The titanium within means the stainless steel is intergranular corrosion resistant after heating between 425 900 degrees celsius.
321 stainless sheet.
For service temperatures up to about 1600 f a stabilizing treatment at 1550 1650 f air cool may be used to provide optimum resistance to intergranular corrosion and to polythionic acid stress corrosion cracking.
Type 321 is a good choice for applications where heat is an issue.
These grades are used because they are not sensitive to intergranular corrosion after heating within the carbide precipitation range of 425 850 c.
321 stainless is reinforced with titanium this alloy excels in high temperature environments providing resistance to cracking and corrosion.
This alloy contains chromium nickel and titanium.
321 ss is a titanium stabilized austenitic chromium nickel stainless steel which was developed to provide an 18 8 type alloy with improved intergranular corrosion resistance.
It is furnished with a crimping tool.
This material maintains its corrosion resistance in temperatures up to 1500 f.
The titanium content of 321 stainless steel preserves corrosion resistance around weld points.
321 321 stainless is a titanium stabilized grade commonly used for service in the 1000 1600 f temperature range.
Type 321 is a good choice for applications where heat is an issue.
321 stainless steel coil and sheet is part of the austenitic family of stainless steel.
Type 321 is a stabilized stainless steel which offers as its main advantage an excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800 to 1500 f 427 to 816 c.
321 is basically a 304 grade containing a stabilizer of titanium.
Foil is often used as a heat treating wrap in temperatures up to 2600 f.
Grades 321 and 347 are the basic austenitic 18 8 steel grade 304 stabilized by titanium 321 or niobium 347 additions.
This material is stabilized against chromium carbide formation by the addition of titanium.
321 stainless steel plates are part of the austenitic family of stainless steel.
It is used principally for applications involving welding or sustained elevated temperature operations.
Stainless steel sheet plate 321 is normally used for aerospace thermal electrical and structural applications.
321 is basically a 304 grade containing a stabilizer of titanium.
321 can be used in applications up to 900 degrees celsius where 304 is normally used up to 500 degrees celsius.
Remarkably high strength as well as scaling resistance and phase stability set 321 stainless steel apart from other similar grades.
321 can be used in applications up to 900 c where 304 is normally used up to 500 c.